Ofertas
|
Masillas de poliéster, 2 componentes
|
thixotropic 2 component filler, polyester resin with BPO hardener, amine accelerator; density: approx. 1.85 g/cm³, fills extremely well, sands and polishes extremely well, hardens to a grey colour, mixing ratio of resin to hardener is 100:2 - 100:3, working life is approx. 4 minutes, can be polished after 15 minutes, shelf life ...
great filling capacity
|
|
thixotropic 2 component filler, polyester resin with BPO hardener (colourless), amine accelerator, density: approx. 1.8 g/cm³, very low pore volume, sands and polishes extremely well, cures to a cream white colour, mixing ratio of resin to hardener is 100:1 - 100:3, working life at 20 °C is approx. 4 minutes, can be sanded ...
very fine surface
|
|
2 component filler paste, polyester resin with BPO hardener (colourless), amine accelerator; density: approx. 0.7 g/cm³, machines down well, cures to an antique white colour, mixing ratio of resin to hardener is 100:2 - 100:4, working life at 20 °C is approx. 5 minutes (2% hardener), can be worked on after 20 - 30 minutes, ...
very lightweight
|
|
|